| STYLE# |
13009 |
|
|
| |
|
|
|
|
|
|
|
| DESCRIPTION / CONSTRUCTION |
|
| |
|
|
| D/C NITRILE/NYLON
CURED |
|
|
|
| AREAS OF APPLICATIONS |
|
| |
|
|
| diaphragm Material |
|
|
| CHARACTERITICS / PHYSICAL PROPERTIES |
|
| |
|
|
| TEST
/ METHOD |
|
Federal Standard 191A or ASTM |
|
REQUIREMENT |
|
|
| Finished
Weight {Oz. / Sq. Yd.} |
|
Method ASTM D-751 |
|
11.0 to 13.0 {min. to
max.} |
|
| Finished
Gauge {Inches} |
|
Method ASTM D-751 |
|
0.012 to 0.014 {min. to
max.} |
|
| Finished
Width {Inches} |
|
Method ASTM D-751 |
|
58" {minimum} |
|
|
| Mullen
Burst {P.S.I.} |
|
Method ASTM D-751 |
|
200 {minimum} |
|
| Adhesion
{Lbs. / Inch} |
|
Method ASTM D-751 |
|
5.0 {minimum} |
|
|
|
|
|
|
|
|
| |
|
|
|
|
|
|
|
|
|
| |
|
|
|
|
|
|
|
| |
|
|
|
|
|
|
|
|
| The
rubber compound used in this product has been investigated and found by
Underwriter Laboratories to be |
|
|
| suitable
for use in UL 157, UL 144, and UL 429. The rubber compound has also been
investigated and found to |
|
|
| comply
with addendum 66 of UN regulation 67 Uniform Provisons Concerning the
Approval of Specific Equipment |
|
|
| of
Motor Vehicles Using Liquefied Petroleum Gasses in their Propulsion System. |
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|